Didymium – UV
and Visible Wavelength reference materials
|
|
|
Product
Description:
Didymium glass has been used for many years as a high
wavelength visible reference material. When prepared in perchloric acid,
didymium gives a spectral scan containing a series of sharp characteristic
peaks that extend well above the useable range of the holmium into the near
NIR (680-900 nm). Again, like holmium, these values are dependent and will
vary with the spectral bandwidth of the measuring instrument.
(see MSDS)
RM-DL:
Consists of one sealed cell, with certified
peak at spectral bandwidth values of 0.10 nm, 0.25 nm, 0.50 nm, 1.00 nm,
1.50 nm, 2.00 nm and 3.00 nm. |
Didymium
- UV and Visible Wavelength
Description:
Didymium (neodymium & praesodymium) in perchloric acid.
Primary
Usage:
Assessment of wavelength scale accuracy
in both UV and visible regions.
Useable
range: 290
nm to 870 nm, instruments with SBW of less than 5 nm.
Physical
Configuration:
Far UV quartz cells that have been permanently heat sealed.
|
| Typical
values obtained: |
| SBW |
nm |
nm |
nm |
nm |
nm |
nm |
nm |
nm |
nm |
nm |
nm |
nm |
nm |
nm |
| 0.10 |
864.35 |
799.18 |
794.14 |
740.06 |
731.57 |
575.19 |
521.82 |
511.81 |
481.65 |
468.78 |
444.05 |
353.83 |
328.92 |
298.24 |
| 0.25 |
864.32 |
799.63 |
794.16 |
740.08 |
731.57 |
575.14 |
521.81 |
511.83 |
481.64 |
468.80 |
444.06 |
353.82 |
328.99 |
298.25 |
| 0.50 |
864.32 |
799.63 |
794.12 |
740.02 |
731.56 |
575.12 |
521.76
|
511.85 |
481.63
|
468.76 |
444.04 |
353.81 |
328.74 |
298.24 |
| 1.00 |
864.40 |
798.99 |
794.08
|
740.04 |
731.63
|
575.04
|
521.56
|
511.87 |
481.67 |
468.66 |
444.01 |
353.80 |
328.78 |
298.29 |
| 1.50 |
864.34 |
799.83 |
794.09 |
740.02 |
731.74 |
574.87 |
521.38 |
511.90 |
481.70 |
468.61 |
443.96 |
353.82 |
328.79 |
298.51 |
| 2.00 |
864.37 |
799.63 |
794.09 |
740.17 |
731.92 |
574.87 |
521.38 |
511.90 |
481.70 |
468.48 |
443.88 |
353.83 |
328.82 |
298.52 |
| 3.00 |
864.37 |
799.63 |
794.09 |
740.34 |
732.48 |
574.98 |
521.38 |
511.57 |
481.64 |
468.25 |
443.73 |
353.53 |
328.84 |
298.79 |
|
All
Starna® didymium Certified Reference Materials are manufactured using
procedures similar to those used in the preparation of our Holmium
Oxide Reference Material (RM-HL). After filling under controlled conditions,
the cells are then permanently sealed by heat fusion and the values
certified by the procedure described below.
Calibration procedure
Traceability:
• Primary instrumental wavelength calibration
is established using the emission lines from mercury and deuterium
sources.
•Additional traceability links to NIST primary materials are established
using SRM 2034 holmium oxide (4% m/v) in perchloric acid (10% v/v).
|
 |
|

|
|
Use:
• All appropriate fundamental parameters and procedures
relating to measurement, handling and storage are fully documented
on the certificate supplied with each Certified Reference Material.
|
|
Cells